"Use Of Zinc Ferrite as A Photocatalyst For Degradation of Toluidine Blue"

Priya Parsoya* and Suresh C. Ameta


The photocatalytic activity of ZnFe2O4 was investigated by carrying out the photocatalytic degradation of toluidine blue dye under visible light. ZnFe2O4 was synthesized by precipitation method. The dye solution was exposed to a 200 W tungsten lamp. The degradation rate of the dye was observed by measuring its absorbance at regular time intervals at 630 nm. Effect of various parameters like pH, concentration of dye, amount of semiconductor and intensity of light on rate of degradation was observed. The optimum rate was observed at pH = 9.5; toluidine blue = 2.10 x 10−5 M; zinc ferrite = 0.06 g and light intensity = 60.0 mWcm−2. The rate constant for a typical run was observed as 2.67 x 10−4 sec−1. A tentative mechanism has been proposed for the photocatalytic degradation of toluidine blue in presence of zinc ferrite involving superoxide anion radical as the active oxidizing species


மறுப்பு: இந்த சுருக்கமானது செயற்கை நுண்ணறிவு கருவிகளைப் பயன்படுத்தி மொழிபெயர்க்கப்பட்டது மற்றும் இன்னும் மதிப்பாய்வு செய்யப்படவில்லை அல்லது சரிபார்க்கப்படவில்லை

குறியிடப்பட்டது

  • CASS
  • கூகுள் ஸ்காலர்
  • ஜே கேட் திறக்கவும்
  • சீனாவின் தேசிய அறிவு உள்கட்டமைப்பு (CNKI)
  • CiteFactor
  • காஸ்மோஸ் IF
  • MIAR
  • ரகசிய தேடுபொறி ஆய்வகங்கள்
  • யூரோ பப்
  • பார்சிலோனா பல்கலைக்கழகம்
  • ICMJE

மேலும் பார்க்க

ஜர்னல் எச்-இண்டெக்ஸ்

Flyer